A walk-through of the reflow process

Posted: 25 Feb 2009  Print Version  Bookmark and Share Subscribe

Keywords: Reflow  organic solder protectant  pre-heat soak 

[Summary of tips] The next stage is the pre-reflow dwell zone, where the temperature is held steady for about 50 seconds in order to permit all parts of the board to reach the same temperature. The temperature during the pre-reflow dwell zone is typically between 180°C and 200°C. During this time, medium-temperature activators are rele......
Please login or register with us to view this article>>
 First Page Previous Page 1 • 2
 
 

Comment on "A walk-through of the reflow process"
Comments:  
*  You can enter [0] more charecters.
*Verify code:
 
Highly Recommended Application Notes

Max's Cool Beans

Clive Maxfield Strange modes of transport and other "stuff"

Someone just pointed me at a YouTube video that claims to show the world's first e-powered multicopter flight...

 

Go to top             Connect on Facebook      Follow us on Twitter      Follow us on Orkut